# Self-Leveling Compound and Screeds for Parquet (UNE 56810)

> UNE 56810 requirements for parquet screeds in Madrid: calcium carbide (CM) moisture limits, flatness with self-leveling compound and silane adhesives.

URL: https://www.parksinta.com/en/blog/self-leveling-compound-screed-parquet-installation-une-56810/  
Actualizado: 2026-11-25  

---

- [![Solera cemento antigua](https://www.parksinta.com/wp-content/uploads/2026/03/Solera-cemento-antigua-1200x900.webp)](https://www.parksinta.com/wp-content/uploads/2026/03/Solera-cemento-antigua-1200x900.webp)

The life of a wood floor depends directly on the screed beneath it. Installing over an uneven or sandy base without leveling it first takes its toll quickly: the floor creaks underfoot, flexes like a bellows and ends up coming loose.

## Technical requirements for the screed under the UNE 56810 standard

The Spanish standard UNE 56810 sets the conditions a screed must meet before it takes a hardwood floor. The most important point is surface flatness: as a reference, dips of more than about 3 mm under a 2-meter straightedge, in any direction, are leveled out.

When we find hollows or dips like these, we apply self-leveling compound to get a continuous plane. That way the boards are not left bridging gaps and do not flex every time someone walks on them.

With solid wood flooring on battens, the screed is not leveled with compound. Unevenness in the screed or the floor structure is taken up by the battens themselves, with blocks and shims.

![Estado inicial de solera de mortero degradada con fisuras y restos de adhesivo](https://www.parksinta.com/wp-content/uploads/2026/03/Solera-cemento-antigua-1200x900.webp)

*Source: ParkSinta technical archive. Worn original screed with remains of black adhesive and differences in level.*

![Solera regularizada con imprimación puente y pasta autonivelante continua](https://www.parksinta.com/wp-content/uploads/2026/03/Solera-cemento-regulada-2-1200x900.webp)

*Source: ParkSinta technical archive. Base leveled with self-leveling compound, ready for direct gluing.*

![Secuencia de obra en la calle Cervantes: solera preparada y colocación de un multicapa de roble de gran formato](https://www.parksinta.com/wp-content/uploads/2024/04/IMG_20230830_101628-ANIMATION.gif)

*Source: ParkSinta technical archive. Job on Calle Cervantes, in the Barrio de las Letras: the prepared screed, covered with a green coating, and the large-format engineered oak being laid on top until finished.*

## Residual moisture and mechanical strength of the mortar

Moisture trapped in the screed is the costliest failure in Madrid renovations. In cement screeds, residual moisture must not exceed 2.5% (somewhat less with underfloor heating), and in anhydrite screeds it cannot exceed 0.5%. These values are not checked by eye or with contact meters, but by taking a sample from inside the screed and measuring it with a calcium carbide (CM) moisture meter.

Besides being dry, the screed has to be hard enough to withstand the pull of the wood once it is glued. If the base is sandy and weak, when the oak shrinks in winter because of the heating, it pulls on the adhesive and tears off the surface crust of the cement, leaving the pieces loose.

## Common defects when installing over a poor base

If a floor is installed over an uneven screed without leveling, mechanical problems show up soon. In floating floors, the voids under the boards cause the bellows effect: the wood gives underfoot and ends up breaking the tongues of the tongue-and-groove joints, with annoying creaks.

In floors glued directly, a weak or sandy screed means the adhesive tears off the mortar surface as soon as the wood starts to pull. The pieces come loose, sound hollow when you walk on them and force whole sections to be lifted.

On ground floors or basements in contact with the ground, moisture rising by capillary action passes through the mortar if there is no barrier. The water enters through the underside of the boards, darkens the wood through a tannin reaction and ends up lifting the floor.

As a workshop rule, on ground floors or street-level premises we apply a two-component epoxy primer broadcast with silica sand. This barrier stops moisture rising from the ground and leaves a rough surface that the self-leveling compound can grip.

## ParkSinta preparation and leveling protocol

On our jobs we prepare the screed in this order, respecting the drying times of each product:

1. **Grinding the base with continuous extraction:** we remove surface laitance, paint and old glue residue with a grinder connected to a workshop vacuum, without raising dust.
2. **Bonding primer:** we apply resins to regulate the absorption of the base, or an epoxy vapor barrier on ground floors at risk of rising damp.
3. **Pouring the self-leveling compound:** we spread the leveling compound (our standard one is Mapei Ultraplan) and go over it with a spiked roller to remove air bubbles and leave a smooth surface.
4. **Final check:** we respect the compound drying time given by the manufacturer before spreading the silane adhesive; the calcium carbide (CM) moisture reading is taken earlier, on the screed.

### Frequently asked questions about screeds and leveling for parquet

**What is the maximum moisture a screed can have before installing wood?**

The UNE 56810 standard allows up to 2.5% CM in cement screeds (somewhat less with radiant heating). In anhydrite screeds the limit drops to under 0.5% CM (0.3% with underfloor heating, per the German TKB 16 guide), always measured with a carbide moisture meter.

**What happens if self-leveling compound is not applied on an uneven floor?**

Dips of more than 3 mm cause flexing and creaking in floating floors, damaging the tongue-and-groove joints. In glued parquet, air pockets prevent the adhesive from bonding fully, leaving pieces hollow or loose.

**How long does self-leveling compound take to dry before the parquet goes down?**

Rapid-setting self-leveling mortars can take foot traffic after 3 or 4 hours. At thicknesses of 3 to 5 mm they reach the right dryness in 24 to 48 hours, according to the manufacturer’s data sheet for that thickness.

Technical advice on screeds for renovations and projects in Madrid

At ParkSinta we carry out technical assessment of screed flatness, surface strength and moisture before any [wood flooring or parquet installation in Madrid](https://www.parksinta.com/en/solid-wood-flooring-installation-madrid/). For architecture projects or renovations in [professional spaces](https://www.parksinta.com/en/commercial-wood-flooring-madrid/), call us at +34 91 543 90 62. A similar case: [Chevron parquet installation – Ultramate oak](https://www.parksinta.com/en/projects/oak-chevron-parquet-installation-ultra-matte/).

[Specification and Professional Spaces](https://www.parksinta.com/en/commercial-wood-flooring-madrid/)
 [📞 +34 91 543 90 62](tel:+34915439062)
 [Book an appointment in Chamberí (Donoso Cortés 24)](https://www.parksinta.com/en/contact/)