# Parquet Finish Hardness: Abrasion and Resistance

> Technical comparison of hardness and wear in parquet finishes: Taber test, scratch resistance, 2K waterborne finishes and our workshop’s criteria in Madrid.

URL: https://www.parksinta.com/en/blog/parquet-finish-hardness-abrasion-scratch-resistance/  

---

- [![Test Taber 1200x1296](https://www.parksinta.com/wp-content/uploads/2016/11/Test-Taber-1200x1296.jpg.webp)](https://www.parksinta.com/wp-content/uploads/2016/11/Test-Taber-1200x1296.jpg.webp)

When planning a wood floor, asking for the hardest finish is usually the first reaction to avoid fast wear. However, looking for the mineral rigidity of ceramic tile in a wood floor is a common mistake from the start. Wood is a living material that moves with changes in humidity, so a film that is too rigid ends up cracking at the first impact or concentrated blow.

## Strength of the board versus elasticity of the finish

In a hardwood floor two different defenses live together, each with its own job. The wood board itself resists knocks and the concentrated weight of furniture, preventing dents. The finish film, for its part, protects the top face against the wear of daily foot traffic, the grit that comes in on shoes and accidental spills of liquids.

In the Madrid winter, heating dries out the air and drops the relative humidity below 30%, making the wood shrink. For this reason the finish must not only be hard on the surface but also keep its elasticity, so it follows the movement of the board without breaking at the pores or losing adhesion.

![Máquina de ensayo Taber para medir resistencia a la abrasión en barnices de parquet](https://www.parksinta.com/wp-content/uploads/2016/11/Test-Taber-1200x1296.jpg.webp)

*Source: ParkSinta technical archive. Taber test: a rotating specimen under abrasive wheels to quantify the wear of the film from continuous friction.*

## Standardized test methods: Taber, Wolff-Wilborn and chemical resistance

In the laboratory, the resistance of a wood finish is not measured with a single figure but with a set of standardized UNE and ISO tests. These tests separately assess wear from friction, surface scratching, elasticity under impact and resistance to household stains:

| Property tested | Test standard | Measurement method | Workshop requirement |
| --- | --- | --- | --- |
| Abrasion resistance | UNE-EN 13696 | Mass loss after 1,000 Taber cycles | < 15 mg in two-component (2K) finishes |
| Scratch resistance | ISO 15184 | Wolff-Wilborn pencil hardness (H scale) | Values between 2H and 3H with elastic memory |
| Impact resistance | UNE-EN 13696 | 500 g steel ball dropped from 120 cm | No cracks around the impact and no detachment |
| Chemical resistance | UNE-EN 13442 | Contact with household reagents for 24 hours | Grade 5 (no rings, swelling or change in sheen) |

## Finish technologies: 2K formulations versus traditional systems

Two-component (2K) waterborne polyurethane finishes are today the reference solution on demanding jobs and high-traffic spaces. Because the hardener is added to the mix before application, the finish cures into a tough, elastic film. It is also free of harsh odors and carries the EMICODE EC1 Plus environmental certification.

For bedrooms or residential rooms with light traffic, one-component (1K) finishes give balanced, easy-going performance. At the other extreme, the old solvent-based urea-formaldehyde finishes are completely ruled out in our workshop because of their glass-like brittleness and their toxic emissions.

![Comparativa visual entre poliuretano al agua y poliuretano al disolvente en roble](https://www.parksinta.com/wp-content/uploads/2009/07/Poliuretano-Disolvente-vs-Poliuretano-al-Agua-2-1200x675.jpg.webp?v=20260602imgfix)

*Source: ParkSinta technical archive. Workshop comparison: oak protected with natural 2K waterborne polyurethane next to the yellowed aging of a solvent-based finish.*

## Application protocol and spread rate in the workshop and on site

The best finish on the market loses its effectiveness if the spread rate is skimped or if the previous sanding does not leave the pores just right. At ParkSinta we always apply one sealer coat and two full coats of 2K polyurethane. We keep a controlled consumption of 100 to 120 grams per square meter for each coat.

With that spread rate we get a continuous film of more than 100 microns that protects the wood against daily traffic. Drying allows walking on it in socks 24 hours after the last pass, and the finish reaches full cure and maximum hardness after one week.

![Restauración de parquet noble con acabado de poliuretano al agua 2K](https://www.parksinta.com/wp-content/uploads/2019/07/Marqueteria-Bona-Traffic-HD-Satinado-1200x659.jpg.webp)

*Source: ParkSinta technical archive. Marquetry floor restored in Madrid with three coats of heavy-duty 2K waterborne polyurethane.*

Specifying high-traffic finishes for architecture and one-off projects

At ParkSinta we advise interior designers and builders on specifying finishes for theaters, hotels and [commercial spaces](https://www.parksinta.com/en/commercial-wood-flooring-madrid/) in Madrid. To assess the requirements of your project or arrange a technical appointment in Chamberí, call us at +34 91 543 90 62.

[Specification and Commercial Spaces](https://www.parksinta.com/en/commercial-wood-flooring-madrid/)
 [📞 +34 91 543 90 62](tel:+34915439062)