# Ipe Exterior Decking Restoration in Madrid

> Restoration and oiling of Ipe exterior decking around pools and terraces in Madrid. UV treatment, rotary cleaning and yearly maintenance.

URL: https://www.parksinta.com/en/blog/ipe-pool-deck-sanding-repair-oiling/  

---

- [![Tarima Exterior IPE Piscina - Lijado, reparación y aceitado](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230331_082103-scaled-scaled.jpg.webp?v=20260602imgfix)](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230331_082103-scaled-scaled.jpg.webp?v=20260602imgfix)

![Tarima exterior de Ipé alrededor de una piscina, vista desde arriba después del lijado y el aceite](https://www.parksinta.com/wp-content/uploads/2023/05/tarima-ipe-piscina-restaurada-hero.webp)

*Source: ParkSinta technical archive. The Ipe pool deck seen from above after sanding and oiling.*

This **Ipe** exterior deck surrounds a swimming pool in Madrid. After many Madrid summers it had gone gray, not red, and some boards had small damage. In spring 2023 we sanded it with many passes, above all between the metal posts that fence the pool. Some boards were also repaired, and the deck got several coats of a Bona exterior oil.

Ipe ( *Handroanthus spp.*) is a very dense wood, about 1,050 kg/m³. Its natural durability is class 1 under UNE-EN 350, the highest against fungi. Even so, without maintenance, sun and pool water turn it gray.

## Why the wood grays and how it behaves outdoors

Constant exposure to sunlight causes an unavoidable photochemical process: ultraviolet rays break down the lignin in the surface layers of the wood. Combined with the chlorinated or salt water of the pool, the tannins and natural oils at the surface are washed out. That is how the grayish patina appears and the surface turns rough.

The graying is only on the surface and does not affect the soundness of the solid Ipe. But unprotected wood collects ground-in dirt and microorganisms, and the rough surface can raise small splinters underfoot when walking barefoot.

![Tarima exterior de Ipé junto a una piscina con valla de postes blancos, antes del aceite](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230329_090649-scaled.jpg.webp?v=20260602imgfix)

*Source: ParkSinta technical archive. The deck beside the pool before oiling.*

![Tarima exterior de Ipé aceitada junto a una piscina, con tumbonas apiladas](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230424_095209-scaled.jpg.webp?v=20260602imgfix)

*Source: ParkSinta technical archive. The deck already oiled, with the sun loungers stacked by the fence.*

## Stages in the restoration of this deck

The work on this pool had three parts:

- **Sanding:** many passes of sandpaper until the gray was gone, above all between the metal posts that fence the pool.
- **Repairs:** the boards with small damage were fixed.
- **Exterior oil:** several coats of a Bona exterior oil. Since it is a non-film-forming product, it does not build a crust or flake, and the wood got its reddish tone back.

![Pasillo de tarima de Ipé entre una valla de postes blancos y el borde de una piscina, antes del aceite](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230329_121954-1-scaled.jpg.webp?v=20260602imgfix)

*Source: ParkSinta technical archive. The walkway between the posts and the pool, before oiling.*

![Pasillo de tarima de Ipé aceitada entre el césped y una valla de postes blancos](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230331_082131-scaled-1200x2541.jpg.webp)

*Source: ParkSinta technical archive. The walkway on the lawn side, beside the row of fence posts, already oiled.*

![Tarima de Ipé aceitada junto al borde de una piscina](https://www.parksinta.com/wp-content/uploads/2023/05/IMG_20230331_082103-scaled.jpg.webp?v=20260602imgfix)

*Source: ParkSinta technical archive. The oiled deck beside the edge of the pool.*

## Frequently asked questions about caring for Ipe exterior decking

**Why does Ipe exterior decking turn gray over time?**

Ultraviolet radiation from the sun breaks down lignin (the natural polymer that binds the cellulose fibers of the wood), while rain and pool water wash out the surface extractives. This causes surface oxidation that turns the wood ash gray, without meaning that the inner structure is damaged or rotten.

**Why should varnish not be applied to an exterior wood deck?**

Varnish forms a rigid, sealed surface film. As the wood expands and contracts under the strong Madrid summer sun, that film cracks, flakes and traps moisture underneath. Outdoors you should always use non-film-forming, open-pore water-repellent penetrating oils or saturators.

**How often does an Ipe deck in Madrid need maintenance?**

There is no fixed interval: it depends on the sun and on how each area is used. The sign is the color. When the wood starts to gray, it is time for another coat of oil, ideally in spring, before the swimming season.

### Exterior deck restoration in Madrid

Before giving a quote we look at the deck on site: which boards need repair and how much sanding is needed. A similar case: [the exterior deck of a penthouse next to the Bernabéu](https://www.parksinta.com/en/blog/outdoor-decking-restoration-oiling-madrid/), repaired, sanded and oiled with two coats of Bona Deck Oil.

[Quote for exterior decking](https://www.parksinta.com/en/contact/)