# How Many Times Can Parquet Be Sanded?

> How many times can a parquet or solid wood floor be sanded? Usable thickness needed in strip parquet, boards on battens and engineered flooring to keep the floor.

URL: https://www.parksinta.com/en/blog/how-many-times-sand-parquet-solid-wood-floor/  

---

- [![Parquet demasiado lijado o fino](https://www.parksinta.com/wp-content/uploads/2014/10/Parquet-demasiado-lijado-o-fino-scaled.jpg)](https://www.parksinta.com/wp-content/uploads/2014/10/Parquet-demasiado-lijado-o-fino-scaled.jpg)

There is a widespread belief that parquet has to be sanded every ten years. The life of a floor is not measured in years, but in the millimeters of wood left above the tongue, the nail or the adhesive. Each sanding takes away part of it and limits the restorations still to come.

To know how many sandings a floor has left, you need to know how it is built and how much wood it still has. You look at the edge of a board wherever you can, for example at a threshold or by removing a baseboard. If you cannot, you ask how old the floor is and how many times it has been sanded, and you test the sound: it gives a good hint of the thickness, without being conclusive.

## Usable thickness: what decides how many times it can be sanded

The usable thickness is the wood between the surface you walk on and the first thing that cannot be sanded. That limit is the tongue of the tongue and groove, the nail head or the layer of adhesive. What a sanding removes depends on the species and on how level the floor is. On a flat floor about 0.8 mm is enough to take off the old finish. If there are lips between pieces or uneven boards, you have to take off 3 mm or more to get the surface flat.

With a badly adjusted machine, or by overusing coarse grit on a floor that was already flat, you wear away wood that did not need removing. That shortens the life of the floor and brings it closer to the point where it breaks. That is why the hand of the tradesman and the adjustment of the drum count as much as the starting thickness.

![Parquet de roble agotado por los lijados, con una pieza rota que deja ver la solera](https://www.parksinta.com/wp-content/uploads/2014/10/Parquet-demasiado-lijado-o-fino-1200x675.jpg.webp)

*Source: ParkSinta technical archive. Oak parquet sanded to the end: in one piece the wood has broken through and the white screed shows.*

## Why the first sanding does not count the same

On a new glued parquet floor, the first sanding serves to level the small differences between strips and prepare for the finish. It usually removes less wood than a restoration, because there is not yet an aged finish to take off or wear from use to even out.

In a restoration you have to remove finish, stains, marks, unevenness and old repairs, and the sanding is more demanding. That is why two floors with the same starting thickness can last very differently.

## Where the limit lies in each floor

In glued solid parquet, whether strip parquet (lamparquet) or thicker strips, there is no tongue: the limit is the layer of wood left above the adhesive. How many sandings it can take depends on that thickness and on how much has been sanded before, so we do not give a general figure: it is checked on each floor.

Thin strip parquet, 8 to 10 mm, takes few: if it loses a lot of thickness, it comes loose or curls at the ends. On thicker parquet, the limit is sometimes set not by the wood but by the height difference that builds up at doors, frames and baseboards.

Solid wood flooring nailed to battens is 22 mm in its standard thickness, but not all of it can be sanded: the tongue of the tongue and groove and the nails set the limit. Above them there are 7 to 9 mm of wood, enough for 4 or 5 sandings; with other thicknesses it varies. Below 2 or 3 mm above the tongue the floor can barely be restored.

On a floating wood floor or an engineered parquet floor only the top wear layer is sanded. The other layers give stability, but they are not the wood you see. Standard 14 mm engineered flooring usually takes one sanding, and two with great care; 20 mm flooring, with a 6 mm wear layer, takes three or more. More detail in [can a floating floor be sanded?](https://www.parksinta.com/en/blog/can-you-sand-and-refinish-engineered-wood-floors/)

Industrial parquet, with the strips laid on edge, takes more than five. Since it is glued, the limit is again the wood left above the adhesive.

## How many sandings each floor can take

These are typical values for each type of floor. On site, what is measured in each case is what counts.

| Floor | Total thickness | Usable wood | Sandings | What to watch |
| --- | --- | --- | --- | --- |
| Glued solid parquet (strip parquet and strips) | From 8 to 14 mm | The layer of wood left above the adhesive | No general figure: assessed on each floor | The 8–10 mm type comes loose or curls if it loses a lot of thickness; on thicker parquet, the height difference with doors and baseboards |
| Solid wood flooring on battens | 22 mm (from 18 to 30 mm) | From 7 to 9 mm above the tongue (varies with other thicknesses) | From 4 to 5 on 22 mm boards | Set the nails below the surface before running the machine; with less than 2–3 mm above the tongue it can barely be restored |
| Standard engineered flooring | 14 mm | From 3 to 4 mm of wear layer | 1, and 2 with great care | Fine sanding, no aggressive grits |
| 20 mm engineered flooring | 20 mm | 6 mm of wear layer | 3 or more | Check the wear layer before sanding |
| Industrial parquet (strips on edge) | Depends on the floor | The wood left above the adhesive | More than 5 | The same as for glued parquet |
| Floor already heavily sanded | — | The core, the nails or the tongues show through | None without repairing first | Open joints or loose pieces: repair, fill with wood slivers or replace pieces |

## Signs that a floor has reached its sanding limit

On visits to apartments in Chamberí and the Salamanca district we often see floors that can no longer take another pass of the machine. The clearest sign is cracks along the board that line up with the tongue and groove. When you step on it, the wood gives a little and creaks, because the upper lip of the groove has lost thickness.

Another warning is nail heads flush with the wood on boards laid over battens: if the machine runs over them, it tears the sandpaper. In these cases sanding is not advisable, and we propose filling the open joints with wood slivers, repairing by areas or replacing the boards; we explain it in [cracks and open joints in parquet](https://www.parksinta.com/en/blog/preventing-wood-floor-cracks-madrid-dry-climate/).

![Tarima de pino lijada con el machihembrado partido y clavos a la vista](https://www.parksinta.com/wp-content/uploads/2014/10/Clavo-Machihembrado-roto-tarima.jpg.webp)

*Source: ParkSinta technical archive. Pine boards sanded to the limit in this area: the nails and the broken tongue and groove are visible.*

![Junta abierta y sucia entre dos tablas de una tarima de pino melis barnizada](https://www.parksinta.com/wp-content/uploads/2014/10/Grieta-tarima-parquet-1-scaled-1200x900.jpg.webp?v=20260602imgfix)

*Source: ParkSinta technical archive. Varnished pitch pine boards with an open joint: before sanding, the joint has to be filled with wood slivers or boards replaced.*

## When to recoat instead of sanding

If the finish is worn but the wood has no deep stains or unevenness, a [recoat](https://www.parksinta.com/en/blog/recoating-parquet-without-sanding/) can be considered. It is more conservative because it removes no wood, it only abrades the old finish, but it requires that finish to be sound, clean and free of wax.

With waxes, silicones, incompatible maintenance products, deep stains, moisture or poor adhesion, the recoat fails. In those cases you have to sand, repair or change the approach.

### Frequently asked questions

**How much wood has to be left to be able to sand?**

On a nailed floor, below 2 or 3 mm of wood above the tongue, restoration is barely viable. In glued parquet, marquetry tiles and panels, the limit is the layer of visible wood above the base, and it is assessed on each floor.

**What can be done if the parquet no longer has enough thickness to sand?**

If the floor is firm and the old finish is intact and free of wax, it can be abraded and given a new coat without removing wood: that is a [recoat](https://www.parksinta.com/en/blog/recoating-parquet-without-sanding/). If there are breaks or worn-out pieces, those areas are repaired or the pieces replaced.

**Does the hardness of the wood affect how often it needs sanding?**

As for how often, yes: a hard wood marks less and takes longer to need another sanding. The number of sandings it can take is set by the thickness it has left, not by hardness; the hardness of each wood is on the [Brinell scale](https://www.parksinta.com/blog/escala-de-la-dureza-de-las-maderas-escala-brinell-2/).

Thickness measurement and technical advice in Madrid

Before giving a quote we check how much wood your floor has left and how many sandings it can take. If it no longer has enough for another, we tell you what can be repaired, recoated or replaced.

[Parquet restoration and sanding](https://www.parksinta.com/en/hardwood-floor-sanding-madrid/)
 [📞 +34 91 543 90 62](tel:+34915439062)
 [Book an appointment in Chamberí (Donoso Cortés 24)](https://www.parksinta.com/en/contact/)